一般在環氧地坪漆施工后的一段時間有些施工后的無錫環氧地坪漆涂膜會產生與基層之間的附著力出現問題,其會使涂層小片脫離或者是與地面的整體脫離。出現這樣的現象往往是無錫固化劑地坪漆廠家在環氧地坪漆施工時有許多因素沒注意造成的。
Generally, after the construction of epoxy floor paint for a period of time, some of the epoxy floor paint film after construction will produce adhesion problems with the base layer, which will make the coating patches or the overall separation from the ground. This phenomenon is often caused by many factors neglected by epoxy floor paint manufacturers in the construction of epoxy floor paint. 其主要原因有以下:
The main reasons are as follows:
1、在施工前進行場內預處理不當,地面還有其余雜質如油污,水溶解物,銹跡等,施工環境清理不干凈。
1. The improper pretreatment before construction and other impurities on the ground, such as oil, water soluble substances, rust, etc., make the construction environment unclean.
2、其中一個在預處理時到環氧地坪漆施工時的間隔時間過長,導致灰塵雜質繼續出現在地表面。
2. The interval between pretreatment and epoxy floor paint construction is too long, which leads to dust impurities continuing to appear on the surface.
3、還有就是在處理時地面的沒有干好就開始進行施工操作。需知如果在潮濕的地面上進行施工,就會有環氧地坪漆層脫離地面的風險存在。
3. There is also the construction operation that starts when the ground is not well done. It is necessary to know that if construction is carried out on wet ground, there will be a risk that the epoxy floor paint layer will break away from the ground.
4、地面材料基底與環氧地坪漆涂層結合不理想,原因是由于基地材料光滑程度比較高,不易與其附著,這其中也可能是環氧環氧地坪漆的涂料配置不適當,這需要根據當地環境因素來進行配置。
4. The combination of the base material and the epoxy floor paint coating is not ideal. The reason is that the base material is not easy to adhere to because of its high smoothness. It may also be that the coating configuration of the epoxy floor paint is inappropriate, which needs to be configured according to local environmental factors.
5、沒有對地面層做烘干處理,或者烘干處理不足,導致環氧環氧地坪漆廠家在進行環氧地坪漆施工時出現涂層不穩定脫落的現象。
5. There is no drying treatment for the surface layer or insufficient drying treatment, which results in unstable peeling of the epoxy floor paint during the construction of the epoxy floor paint by the epoxy floor paint manufacturer.
防范措施:
Preventive measures:
1、環氧地坪漆廠家對即將進行施工的環氧地坪進行表面的清理,如遇到光滑程度較高的地面則用噴砂,或用砂質對其進行處理,使其粗糙度增強,方便施工。
1. The epoxy floor paint manufacturer cleans the surface of the epoxy floor which is going to be constructed. If it encounters the surface with higher smoothness, it will be treated with sand blasting or sand, so as to enhance its roughness and facilitate construction.
2、在處理好等地面風干不能過長,一般都是3-4個小時左右,就要開始施工。也可以同時對地面進行干燥處理。
2. The ground air-drying can not be too long when it is well handled. Generally, it takes about 3-4 hours to start construction. The ground can also be dried at the same time.
3、無錫固化劑地坪地坪漆廠家在無錫環氧地坪漆施工時要選擇好與其基層地質適合度高的材料,要保證其附著力能夠適應其地面的材質。
3. Floor paint manufacturers should choose materials with high geological suitability with their base when constructing epoxy floor paint, and ensure that their adhesion can adapt to the material of their floor.